Guide · 5 min read

Substrates for 2D materials

Why 90 nm and 285 nm SiO₂ on P++ silicon, when to use sapphire, and how to keep flakes clean.

Graphene, MoS₂, WSe₂ and other 2D crystals are only one or a few atoms thick, so the substrate decides whether you can see them, contact them and gate them.

Seeing flakes: oxide thickness

A thin flake on SiO₂/Si changes the interference colour of the oxide. For graphene the contrast under white or green light is strongest for oxide thicknesses around 90 nm and 285 – 300 nm, which is why these two values became the standard. Other thicknesses work, but monolayers become much harder to find.

Gating: P++ silicon

On heavily doped (P++, 0.001 – 0.005 Ω·cm) silicon the substrate itself is the gate electrode, so you can tune carrier density without extra fabrication. Thinner oxide (90 nm) gives a stronger gate effect for the same voltage; thicker oxide (285 nm) tolerates higher voltages.

Growth: sapphire

CVD growth of transition-metal dichalcogenides is commonly done on C-plane sapphire, which is inert at growth temperatures and can promote aligned domains. Grown films can then be transferred onto SiO₂/Si for devices.

Encapsulation: hBN

Hexagonal boron nitride is atomically flat and free of dangling bonds. Sandwiching a flake between hBN layers improves mobility and protects air-sensitive materials.

Keeping surfaces clean

  • Clean SiO₂/Si with solvents, then a short oxygen plasma, immediately before exfoliation.
  • Pre-diced 10 × 10 mm chips avoid cleaving debris.
  • Use shadow masks or pre-patterned markers to locate flakes later.

See thermal oxide wafers, including 90 nm and 285 nm on P++ silicon.

Not sure which configuration you need?

Tell us about your process, instrument or experiment. A materials specialist will recommend the right substrate, grade or tool, and quote it.

Talk to an expert