Ratgeber · 5 Min. Lesezeit

Substrate für 2D-Materialien

Warum 90 nm und 285 nm SiO₂ auf P++-Silizium, wann Saphir sinnvoll ist und wie Flocken sauber bleiben.

Technische Spezifikationen und Fachartikel sind auf Englisch.

Graphene, MoS₂, WSe₂ and other 2D crystals are only one or a few atoms thick, so the substrate decides whether you can see them, contact them and gate them.

Seeing flakes: oxide thickness

A thin flake on SiO₂/Si changes the interference colour of the oxide. For graphene the contrast under white or green light is strongest for oxide thicknesses around 90 nm and 285 – 300 nm, which is why these two values became the standard. Other thicknesses work, but monolayers become much harder to find.

Gating: P++ silicon

On heavily doped (P++, 0.001 – 0.005 Ω·cm) silicon the substrate itself is the gate electrode, so you can tune carrier density without extra fabrication. Thinner oxide (90 nm) gives a stronger gate effect for the same voltage; thicker oxide (285 nm) tolerates higher voltages.

Growth: sapphire

CVD growth of transition-metal dichalcogenides is commonly done on C-plane sapphire, which is inert at growth temperatures and can promote aligned domains. Grown films can then be transferred onto SiO₂/Si for devices.

Encapsulation: hBN

Hexagonal boron nitride is atomically flat and free of dangling bonds. Sandwiching a flake between hBN layers improves mobility and protects air-sensitive materials.

Keeping surfaces clean

  • Clean SiO₂/Si with solvents, then a short oxygen plasma, immediately before exfoliation.
  • Pre-diced 10 × 10 mm chips avoid cleaving debris.
  • Use shadow masks or pre-patterned markers to locate flakes later.

See thermal oxide wafers, including 90 nm and 285 nm on P++ silicon.

Unsicher, welche Konfiguration Sie brauchen?

Erzählen Sie uns von Ihrem Prozess, Gerät oder Experiment. Ein Materialspezialist empfiehlt das passende Substrat, die richtige Qualität oder das passende Werkzeug und erstellt ein Angebot.

Expertenberatung